產(chǎn)品詳情
寧夏斯米克銀焊絲現(xiàn)貨批發(fā)
L312 Wire & rod
絲 595-605 Ag40.Cu.Zn.Cd Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等
L313 Wire & rod
絲 625-635 Ag50.Cu.Zn.Cd Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等 BAg-1a
L321 Wire & rod
絲 615-650 Ag56.Cu.Zn.Sn Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等 BAg-7
L323 Wire & rod
絲 665-755 Ag30.Cu.Zn.Sn Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等
L325 Wire & rod
絲 645-685 Ag45.Cu.Zn.Sn Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等 BAg-36
L326 Wire & rod
絲 650-720 Ag38.Cu.Zn.Sn Brazing of copper, copper alloys, steel and stainless steel etc.
釬焊銅及銅合金、鋼及不銹鋼等 BAg-34
HAG-25BSn,含銀25,等同于美標(biāo)AWS BAg-37,是銀、銅、鋅、錫合金,熔點(diǎn)低于HAg-25B,提高了潤(rùn)濕性和填充性??珊搞~、鋼等材料。熔點(diǎn)680-780攝氏度。
HAG-30B,含銀30,等同于美標(biāo)AWS BAg-20,國(guó)標(biāo)BAg30CuZn ,是銀、銅、鋅合金,熔點(diǎn)稍高,接頭有較好韌性,可釬焊銅、銅合金、鋼等材料。熔點(diǎn)677-766攝氏度。
HAG-35B,含銀35,等同于美標(biāo)AWS BAg-35,是銀、銅、鋅合金,中等熔化溫度,接頭有較好韌性,可釬焊銅、銅合金、鋼等材料。熔點(diǎn)621-732攝氏度。
HAG-35Sn,含銀35,等同于國(guó)標(biāo)BAg34CuZnSn,是銀、銅、鋅、錫合金,中等熔化溫度,有較好的流動(dòng)性,更適用于鐵素體和非鐵素體鋼的焊接。熔點(diǎn)620-730攝氏度。
HAG-40B,含銀40,是銀、銅、鋅、合金,具有較好的流動(dòng)性、滲透性和韌性,熔點(diǎn)677-732攝氏度。
HAG-40BNi,含銀40,是銀、銅、鋅、鎳合金,等同于美標(biāo)AWS BAg-4,具有較好的抗蝕性、適用于不銹鋼的焊接和鎳基合金及炭化鎢的焊接,熔點(diǎn)670-780攝氏度。
HAG-40BSn,含銀40,等同于美標(biāo)AWS BAg-28,是銀、銅、鋅、錫合金,有很好的流動(dòng)性,用于鐵素體鋼和非鐵素體鋼的焊接效果尤其理想,熔點(diǎn)650-710攝氏度。
HAG-45B,含銀45,等同于美標(biāo)AWS BAg-5、國(guó)標(biāo)BAg45CuZn及L303,是銀、銅、鋅、合金,綜合性能好,有優(yōu)良的韌性和滲透性,常用于機(jī)電、食品機(jī)械及表面光潔度要求較高零部件的釬焊。熔點(diǎn)663-743攝氏度。
HAG-45BSn,含銀45,等同于美標(biāo)AWS BAg-36,是銀、銅、鋅、錫合金,性能同45B但熔化溫度比45B低。熔點(diǎn)645-680攝氏度。
HAG-50B,含銀50,等同于美標(biāo)AWS BAg-6、國(guó)標(biāo)BAg